Focus On High-Quality Silicate (Ceramic) Materials

GOWAY Deflocculant / Dispersing Agent Series (4 products)


Time:

2026-08-07

Author:

Source:


GOWAY Ceramic Production Solutions

GOWAY Ceramic Production Solutions

🧪 GOWAY Deflocculant / Dispersing Agent Series 100% STPP Replacement 4 Products
Application: Ceramic Body Recommended Dosage: 0.2% – 0.5% Key Advantage: 30%-40% of STPP Cost Packaging: 25kg/bag | 25kg/drum | IBC
🌀 6 Core Effects on Ceramic Slurry Technical Details
  • 🔹 Significantly Reduces Slurry Viscosity
    Through electrostatic repulsion and steric hindrance, reduces slurry viscosity by 40-60%, enabling high-solid-content slurries to maintain excellent fluidity while greatly reducing pumping energy consumption.
  • 🔹 Increases Solid Content to 65-72%
    At the same fluidity level, solid content increases by 5-8 percentage points compared to traditional STPP formulations, directly reducing spray drying water evaporation and saving energy by 10-15%.
  • 🔹 Improves Slurry Rheological Properties
    Imparts shear-thinning thixotropic behavior — flows smoothly during agitation, remains stable at rest, effectively preventing pipe sedimentation and clogging.
  • 🔹 Extends Slurry Aging Time
    Inhibits microbial growth and particle agglomeration, extending aging time from 24h to 72h+, providing greater production scheduling flexibility and better slurry consistency.
  • 🔹 Increases Ball Mill Efficiency by 8-12%
    Reduces inter-particle friction, allowing grinding media to work more effectively on materials — achieving finer particle size in the same milling time, or reducing milling time to reach the same fineness.
  • 🔹 100% Replacement of Sodium Tripolyphosphate (STPP)
    Completely replaces traditional STPP dispersant with no performance degradation — often superior performance — at only 30%-40% of STPP cost.
💡 Engineering Recommendation: Select the appropriate product grade based on the body formulation (kaolin content, quartz/feldspar ratio). The optimal dosage should be determined through laboratory trials.
📊 Technical Parameters Slurry Preparation
Solid Content 65–72%
Slurry Fluidity 30–60s (Ford Cup #4)
Ball Mill Time 10–14h
Fineness 250 Mesh Residue ≤0.5%
Energy Savings 10–15% Evaporation Reduction
Production Increase +8% ~ +12%
Aging Time 24h → 72h
Viscosity Reduction 40–60%
🎯 Quick Product Selection Guide
• FG-2017 → High Kaolin Formulations
• FG-MK03 → Suspension Improvement
• FG-N203B → Dark/Black Bodies
• FG-SL01A → White/Light Bodies
🎯 Comprehensive Benefits
60-70%
Cost Savings vs. STPP
Deflocculant Cost
10-15%
Spray Drying Energy Reduction
High Solid Content
8-12%
Ball Mill Capacity Increase
More Output in Same Time
40-60%
Slurry Viscosity Reduction
Lower Pumping Energy
100%
STPP Replacement
No Performance Loss
24→72h
Extended Aging Time
Flexible Scheduling